Rhenium (Re) — Element 75
Standard Atomic Weight: 186.21 u · Electronic Configuration: [Xe] 4f14 5d5 6s2
Fundamental Periodic Properties
| Atomic Number (Z) | 75 |
|---|---|
| Chemical Symbol | Re |
| Standard Atomic Weight | 186.21 u (IUPAC CIAAW) |
| Category | Transition metal |
| Group, Period, Block | Group 7, Period 6, d-block |
| Electron Configuration | [Xe] 4f14 5d5 6s2 |
| Electrons per Shell | 2,8,18,32,13,2 |
| Common Oxidation States | +7, +4 |
| State at STP | solid |
| Electronegativity (Pauling) | 1.9 |
| 1st Ionization Energy | 7.834 eV |
| Atomic Radius | 151 pm |
| Crystal Structure | hcp |
Discovery & Historical Context
Discovered: 1925 by Noddack, Tacke & Berg
Name Origin: Latin Rhenus (Rhine)
Everyday Applications & Technological Role
Jet-engine turbine blades, catalysts
Key Scientific Facts
- Rhenium was the last stable element ever discovered, in 1925.
- A dash of rhenium lets jet-engine turbine blades survive infernal heat.
- It melts at 3186 degrees, third highest of all elements.
- Platinum-rhenium catalysts refine the high-octane gasoline in your tank.
- Mass spectrometers ionize samples on white-hot rhenium filaments.
- Almost all of it arrives as a trace byproduct of copper and molybdenum mining.
- It is one of the rarest elements in Earth's crust.