Palladium (Pd) — Element 46
Standard Atomic Weight: 106.42 u · Electronic Configuration: [Kr] 4d10
Fundamental Periodic Properties
| Atomic Number (Z) | 46 |
|---|---|
| Chemical Symbol | Pd |
| Standard Atomic Weight | 106.42 u (IUPAC CIAAW) |
| Category | Transition metal |
| Group, Period, Block | Group 10, Period 5, d-block |
| Electron Configuration | [Kr] 4d10 |
| Electrons per Shell | 2,8,18,18 |
| Common Oxidation States | +2, +4 |
| State at STP | solid |
| Electronegativity (Pauling) | 2.2 |
| 1st Ionization Energy | 8.337 eV |
| Atomic Radius | 139 pm |
| Crystal Structure | fcc |
Discovery & Historical Context
Discovered: 1803 by William Wollaston
Name Origin: Pallas (asteroid)
Everyday Applications & Technological Role
Catalytic converters, hydrogen purification
Key Scientific Facts
- Palladium is named after the asteroid Pallas, spotted just before the metal's discovery.
- It can soak up 900 times its own volume of hydrogen, and lets only hydrogen pass through — perfect for purifying it.
- Catalytic converters are the biggest use of palladium on the planet.
- The 2010 Nobel Prize went to palladium-catalyzed cross-coupling reactions used to build medicines.
- It hides inside multilayer ceramic capacitors in nearly every phone and laptop.
- Dentists use palladium alloys for crowns and bridges.
- Hydrogen fuel-cell research leans on palladium membranes and catalysts.