Zirconium (Zr) — Element 40
Standard Atomic Weight: 91.224 u · Electronic Configuration: [Kr] 4d2 5s2
Fundamental Periodic Properties
| Atomic Number (Z) | 40 |
|---|---|
| Chemical Symbol | Zr |
| Standard Atomic Weight | 91.224 u (IUPAC CIAAW) |
| Category | Transition metal |
| Group, Period, Block | Group 4, Period 5, d-block |
| Electron Configuration | [Kr] 4d2 5s2 |
| Electrons per Shell | 2,8,18,10,2 |
| Common Oxidation States | +4 |
| State at STP | solid |
| Electronegativity (Pauling) | 1.33 |
| 1st Ionization Energy | 6.634 eV |
| Atomic Radius | 175 pm |
| Crystal Structure | hcp |
Discovery & Historical Context
Discovered: 1789 by Martin Klaproth
Name Origin: Persian zargun (gold-colored)
Everyday Applications & Technological Role
Nuclear fuel cladding, fake diamonds (zirconia)
Key Scientific Facts
- Its name comes from the Persian zargun, meaning gold-colored, after the gemstone zircon.
- Nuclear fuel rods wear zirconium-alloy cladding because it barely absorbs neutrons.
- Cubic zirconia, its sparkly oxide, is the classic diamond lookalike in jewelry.
- It resists corrosion so fiercely it is used in chemical plants and surgical implants.
- Martin Heinrich Klaproth identified it in 1789, and Berzelius isolated the metal in 1824.
- Tiny zircon crystals from Australia are the oldest known Earth material, about 4.4 billion years old.
- Dentists craft crowns from yttria-stabilized zirconia, one of the toughest ceramics known.