CHEMVEN

Pulp, Paper and Sugar — Chemistry at Scale

The Kraft process, papermaking, and sugar refining — three giant industries built on applied chemistry.

INDUSTRIALLevel: IntermediateAcademic Reference

Overview & Foundations

Wood is roughly half cellulose, a quarter lignin, the rest hemicellulose and extractives. Kraft pulping cooks wood chips in white liquor (NaOH + Na₂S) at about 170 °C, dissolving the lignin and freeing strong cellulose fibers. The spent black liquor is concentrated and burned in a recovery boiler — which both powers the mill and regenerates the chemicals: green liquor (Na₂CO₃ + Na₂S) is causticized with lime back to white liquor, a near-closed loop that makes most Kraft mills energy self-sufficient.

Papermaking then exploits the cellulose itself: beating fibrillates the fibers, and hydrogen bonds between fibers give paper its strength; sizing agents and mineral fillers (calcium carbonate, clay) control ink absorption and opacity. Sugar refining is a purification cascade — cane or beet juice is limed (CaO) and carbonated (CO₂) to precipitate impurities as CaCO₃, then evaporated and crystallized; raw sugar (~96% sucrose) is washed (affination), re-melted, filtered over carbon, and recrystallized to 99.9% pure white sugar.

Core Chemical Concepts

Governing Formulas & Laws

NaOH + Na₂S
White liquor (Kraft pulping)
CaO + CO₂ → CaCO₃
Carbonatation purification in sugar refining

Worked Numerical Examples

Q: A Kraft mill recovers 97% of its pulping chemicals each cycle. Starting with 1000 t of white-liquor chemicals, how much is lost per cycle?
A: 3% of 1000 t = 30 t lost per cycle, made up with makeup chemicals. That high recovery is what makes Kraft economical and relatively clean.

Industrial & Laboratory Applications

Common Student Misconceptions

Paper is not just pressed wood — residual lignin yellows and weakens it
Brown Kraft bags are unbleached; whiteness needs extra bleaching stages

Everyday Life & Real-World Relevance

Practice & Review Questions

Why is it called 'Kraft'?
German/Swedish for 'strength' — Kraft paper's long fibers are exceptionally strong.
What happens to the lignin?
Burned in the recovery boiler for process energy and chemical recovery.

Scholarly Literature & References

← Back to Industrial Hub · All Encyclopedia Topics