Polymer Fundamentals — Chains, Addition vs Condensation
How monomers become macromolecules, and how chain length is measured.
Overview & Foundations
A polymer is a macromolecule built from repeating units (mers) joined in long chains. Addition polymerization links monomers with C=C double bonds (e.g. ethylene → polyethylene) with no by-product, initiated by radicals, cations or Ziegler–Natta catalysts; condensation polymerization joins bifunctional monomers (e.g. diacid + diol → polyester) with loss of a small molecule such as water, and the chain grows stepwise so high molar mass requires very high conversion.
Chain length is described by averages: the number-average molar mass Mn = ΣNiMi/ΣNi and the weight-average Mw = ΣNiMi²/ΣNiMi. Their ratio PDI = Mw/Mn (polydispersity index) measures breadth — PDI = 1 is perfectly uniform, commercial polymers are 1.5–3. The degree of polymerization DP = Mn / M₀ where M₀ is the repeat-unit molar mass.
Core Chemical Concepts
- Monomer → polymer: addition (chain growth, no by-product) vs condensation (step growth, H₂O lost)
- Mn (number-average), Mw (weight-average), PDI = Mw/Mn ≥ 1
- DP = Mn/M₀ gives the average number of repeat units per chain
- Thermoplastics (melt/reform) vs thermosets (crosslinked, permanent)
Governing Formulas & Laws
AveragesDispersityDegree of polymerizationWorked Numerical Examples
Industrial & Laboratory Applications
- Packaging, fibers, adhesives — polyethylene, PET bottles, nylon
- Molecular-weight control sets mechanical strength and melt viscosity
Common Student Misconceptions
Everyday Life & Real-World Relevance
- Mn/Mw/PDI/DP definitions
- Addition vs condensation — monomers, by-products, kinetics
- Thermoplastic vs thermoset
Practice & Review Questions
Scholarly Literature & References
- Clayden, Greeves & Warren, Organic Chemistry
- NCERT Chemistry, Class XII