Pulp, Paper and Sugar — Chemistry at Scale
The Kraft process, papermaking, and sugar refining — three giant industries built on applied chemistry.
Overview & Foundations
Wood is roughly half cellulose, a quarter lignin, the rest hemicellulose and extractives. Kraft pulping cooks wood chips in white liquor (NaOH + Na₂S) at about 170 °C, dissolving the lignin and freeing strong cellulose fibers. The spent black liquor is concentrated and burned in a recovery boiler — which both powers the mill and regenerates the chemicals: green liquor (Na₂CO₃ + Na₂S) is causticized with lime back to white liquor, a near-closed loop that makes most Kraft mills energy self-sufficient.
Papermaking then exploits the cellulose itself: beating fibrillates the fibers, and hydrogen bonds between fibers give paper its strength; sizing agents and mineral fillers (calcium carbonate, clay) control ink absorption and opacity. Sugar refining is a purification cascade — cane or beet juice is limed (CaO) and carbonated (CO₂) to precipitate impurities as CaCO₃, then evaporated and crystallized; raw sugar (~96% sucrose) is washed (affination), re-melted, filtered over carbon, and recrystallized to 99.9% pure white sugar.
Core Chemical Concepts
- Kraft: NaOH + Na₂S white liquor dissolves lignin at ~170 °C
- Recovery boiler regenerates pulping chemicals
- Paper strength = cellulose–cellulose hydrogen bonding
- Sugar: liming → carbonatation → crystallization → affination
Governing Formulas & Laws
White liquor (Kraft pulping)Carbonatation purification in sugar refiningWorked Numerical Examples
Industrial & Laboratory Applications
- Corrugated packaging and tissue from Kraft pulp
- Dissolving pulp for rayon/viscose fibers
- Refined white sugar; molasses as fermentation feedstock
Common Student Misconceptions
Everyday Life & Real-World Relevance
- White liquor: NaOH + Na₂S; black liquor: spent + dissolved lignin
- Recovery loop: black → green → white liquor
- Affination washes raw-sugar crystals before re-refining
Practice & Review Questions
Scholarly Literature & References
- Clayden, Greeves & Warren, Organic Chemistry
- Housecroft & Sharpe, Inorganic Chemistry