Thermal Analysis: TGA, DSC, DTA
Heat it and watch: mass loss, heat flow and transitions reveal composition and stability.
Overview & Foundations
TGA (thermogravimetric analysis): mass vs temperature — steps reveal decomposition, water loss (hydrates), filler content in polymers, and thermal stability rankings. Derivative (DTG) sharpens overlapping steps.
DSC (differential scanning calorimetry): heat flow vs temperature — measures Tg (glass transition, step), crystallization (exotherm), melting (endotherm), and heat capacity. Purity from melting-point depression; polymer crystallinity from ΔH_fusion.
DTA (differential thermal analysis): temperature difference vs reference — the older cousin of DSC, still used for high-temperature ceramics and phase diagrams. Combined TGA-DSC runs both at once. Evolved-gas analysis (TGA-MS/FTIR) identifies what leaves at each step.
Core Chemical Concepts
- TGA: mass vs T (decomposition)
- DSC: heat flow vs T (transitions)
- Tg, Tm, crystallization from DSC
- Purity via melting depression
- TGA-MS identifies evolved gases
Governing Formulas & Laws
Hydrate formulas from TGAWorked Numerical Examples
Industrial & Laboratory Applications
- Polymer characterization
- Drug stability testing
- Cement/hydrate analysis
Common Student Misconceptions
Everyday Life & Real-World Relevance
- Mass steps = composition
- Heat peaks = transitions
- Rate and atmosphere matter
Practice & Review Questions
Scholarly Literature & References
- Skoog, West, Holler & Crouch, Fundamentals of Analytical Chemistry
- Atkins & de Paula, Atkins' Physical Chemistry