Magnesium fluoride (MgF2)

CAS Registry Number: 7783-40-6 · Standard Molar Mass: 62.30 g/mol

SOLIDCAS: 7783-40-6MW: 62.30 g/mol
Safety Notice: For educational reference only. Always consult the official Safety Data Sheet (SDS).

Chemical & Physical Constants

IUPAC NameMagnesium difluoride
Chemical FormulaMgF2
CAS Registry Number7783-40-6
Molar Mass62.30 g/mol
State of Matter (STP)solid
Melting Point1263 °C
Boiling Point2227 °C
Categorymaterials
GHS Hazard CategoryNon-hazardous

Everyday & Industrial Uses

Anti-reflection coatings on lenses and rugged ultraviolet optics.

Chemical Notes & Behavior

Hard, slightly birefringent fluoride that reaches further into the UV than glass.