Gypsum (CaSO4·2H2O)

CAS Registry Number: 13397-24-5 · Standard Molar Mass: 172.17 g/mol

SOLIDCAS: 13397-24-5MW: 172.17 g/mol
Safety Notice: For educational reference only. Always consult the official Safety Data Sheet (SDS).

Chemical & Physical Constants

IUPAC NameCalcium sulfate dihydrate
Chemical FormulaCaSO4·2H2O
CAS Registry Number13397-24-5
Molar Mass172.17 g/mol
State of Matter (STP)solid
Melting Point
Boiling Point
Categoryindustrial
GHS Hazard CategoryNon-hazardous

Everyday & Industrial Uses

Raw material for plaster of Paris; cement manufacture; soil conditioner.

Chemical Notes & Behavior

Calcium sulfate dihydrate — a soft white mineral; loses its water of crystallization on heating to give the hemihydrate (plaster of Paris).