Cerium(IV) oxide (CeO2)

CAS Registry Number: 1306-38-3 · Standard Molar Mass: 172.12 g/mol

SOLIDCAS: 1306-38-3MW: 172.12 g/mol
Safety Notice: For educational reference only. Always consult the official Safety Data Sheet (SDS).

Chemical & Physical Constants

IUPAC NameCerium dioxide
Chemical FormulaCeO2
CAS Registry Number1306-38-3
Molar Mass172.12 g/mol
State of Matter (STP)solid
Melting Point2600 °C
Boiling Point
Categorymaterials
GHS Hazard CategoryNon-hazardous

Everyday & Industrial Uses

Catalytic converters, glass-polishing powder and solid-oxide fuel cells.

Chemical Notes & Behavior

Ceria stores and releases oxygen by switching between Ce(IV) and Ce(III).